Three ways to take the grain off an SLS or MJF part. Two remove material. One reflows it. The difference matters more than it looks.
Run your thumb over a freshly printed SLS part and you’ll feel it: a fine, sandy grain. It’s the signature of powder-bed printing, and it’s the first thing a customer notices when they pick the part up.
So the question we get most often about finishing isn’t “can you make it smoother?” It’s “which way?”
There are three answers, and they are not interchangeable.
Vibro polishing for SLS and MJF parts: wearing the surface smooth
Vibro polishing, also called vibratory finishing or tumbling, is mechanical. The parts go into a bowl with ceramic, plastic or organic media, and the bowl vibrates for hours. The media rubs the peaks off the surface, a few microns at a time.
It works. UK supplier PDJ Vibro, whose bowls Ogle Models and Prototypes use on SLS nylon, describes the result on flat surfaces and gentle curves as a satin finish, close to a moulded texture, and Ogle reckon it cut their painting prep by about a third. A typical cycle runs 4 to 12 hours, and because the bowl runs unattended and the media is cheap, it is the lower-cost option.

But it works by removing material. In our experience that’s where you need to use judgement. Sharp edges round over. Embossed lettering and thin ribs soften. Ogle’s own guidelines warn that fine mesh is unlikely to survive and that media can lodge inside cavities and never come out. The longer you run it, the smoother it gets, and the more of the part you lose. For a cosmetic housing that’s fine. For a part with a crisp edge, a logo or a thin wall, we don’t recommend it, and we say so.
And the media has to touch the surface. The inside of a duct, the bottom of a deep pocket, the channels of a fluid connector: if a ceramic chip can’t get in, move about and get out again, that surface stays rough.
Vapor Smoothing for 3D printed parts: reflowing and sealing the surface
Vapor smoothing is chemical. We run it in-house on AMT PostPro equipment. Parts sit in a sealed chamber, a solvent is vaporised around them, and the outermost layer of the plastic softens and reflows. The peaks don’t get knocked off; they flow into the valleys.
Three things follow from that.
Nothing is removed. The material is redistributed, not abraded, so dimensions hold and fine detail survives. There are limits (we specify a minimum wall thickness for the process), but you are not slowly sanding the part away.
The surface seals. A reflowed skin is continuous. Water, oil and air that would soak into a porous SLS surface now sit on top of it. That turns a cosmetic treatment into a functional one.
It reaches where the others can’t. Although there are limitations, the gas can reach areas the other two methods can’t.

The finish is closer to injection-moulded than anything mechanical can give you: smooth, slightly glossy, with better colour consistency. We offer it on our own SinterWorx G4, SinterWorx C6 and MJF PA12 or even customer supplied parts.
Hand finishing: the third way
The third option isn’t a machine. It’s a technician, abrasive paper and judgement.
Hand sanding is how we deal with the faces that matter more than the rest of the part. An O-ring groove that has to seal. A mating face that needs to sit flat against something. The windswept surfaces of an F1 part, where the airflow sees every ripple. Those faces get worked individually; everything else stays as printed or goes through Vapor smoothing.
What you get is control. The finish goes exactly where it’s needed, it can be taken smoother and flatter than either machine process will manage, and nothing is touched that didn’t need touching.
What you pay for is the hands. It’s slow, so it costs, and because it depends on the person holding the part it is never quite as repeatable batch to batch as a chamber or a bowl. For ten parts with three critical faces, it’s the right call. For five hundred cosmetic housings, it isn’t.
Vapor Smoothing vs vibro polishing vs hand finishing
| Vapor Smoothing | Vibro Polishing | Hand Sanding | |
|---|---|---|---|
| How it works | Solvent vapor reflows the surface | Media wears the surface away | Technician works chosen faces |
| Finish | Smooth, glossy, moulded look | Smooth, matte to satin | Smoothest and flattest, where applied |
| Material removal | None; redistributed | Yes; edges and fine detail soften | Yes, but only where intended |
| Seals the surface | Yes | No | No |
| Internal and hidden faces | Reached | Only where media can touch | Only where a hand can reach |
| Fine edges and lettering | Preserved | Rounded; mesh and thin walls at risk | Preserved if avoided |
| Consistency across a batch | High | High | Lower; depends on the person |
| Cost | Mid | Lowest | Highest per part |
| Best for | Fluid contact, complex geometry, visible parts | Tactile smoothing, paint prep | Sealing faces, flat mating faces, aero surfaces |
Where it stops being cosmetic
The sealing is the part people underestimate.
We make sonar mount parts for Triton Submersibles in MJF PA12. They go to 1,000 metres on the Triton 3300/3, carrying a 3D imaging sonar for the OceanX team. At that depth a porous surface is not a finish problem, it’s a water-ingress problem. Triton told us that being able to print replacements and variants in days lets them keep the vehicles looking right without holding up critical projects.

The same logic applies closer to home: underwater housings, injection-moulding prototypes that need to behave like the moulded part, handheld devices that get wiped down, automotive trim that’s on show. In every one of those, “smoother” is the wrong spec. “Sealed” is the spec.
Which 3D printing finishing process should you choose?
If you want a part that feels better in the hand, keeps a matte look, has no sharp edges or fine detail to protect, and the budget matters more than the finish, vibro polishing does the job. We don’t offer it ourselves, but if it’s the right finish for your part we’ll tell you, and point you to someone who does.
If the part will see water, oil or air; if it has internal features or sharp detail; or if it needs to pass for a moulding, Vapor smoothing is the one. That’s the process we run, and we’ll tell you when a part isn’t suited to it.
And if only two or three faces matter, say the sealing groove and the surface the air runs over, hand finishing those and leaving the rest alone is often the best answer of the three. Slower, dearer, but the care lands exactly where the part needs it.
Either way, decide the finish when you decide the material and the geometry, not after the part is on the bench. A finish specified from a photograph is how a crisp edge turns into a radius nobody asked for.
Not sure which finish your part needs? Send us the file and the application and we’ll tell you straight.
Frequently Asked Questions
What is the difference between Vapor Smoothing and vibro polishing?
Vibro polishing mechanically removes small amounts of material using abrasive media, producing a smoother matte or satin surface. Vapor Smoothing uses solvent vapour to reflow the outer surface of compatible polymers, creating a smoother, sealed finish without mechanically abrading the component.
Vapor Smoothing seals the surface. Whether the whole part holds a given fluid at a given pressure depends on material, wall thickness and geometry, which is why we agree that requirement with you up front. Pay for sealing and we guarantee the part meets it, or we remake it.
Yes. It removes material, so edges round, lettering softens and thin walls or mesh can fail.
No. It reduces roughness; it doesn’t create a continuous skin.
Yes. Vibratory finishing can be used to reduce the characteristic grainy surface texture of SLS parts. Research by Formlabs on SLS Nylon 11 and Nylon 12 demonstrated reductions in surface roughness of more than 80% after eight hours under its test conditions. Results depend on the equipment, media, material and processing time.
It can be particularly useful for complex parts because it is a non-line-of-sight process. Vapour can interact with surfaces that may be difficult for conventional mechanical finishing methods to reach. Suitability still depends on the material and specific component design.